سٹینلیس سٹیل کیا ہے؟ 347?
سٹینلیس سٹیل 347 is similar to the 321 stainless steels in that it is often used as a stabilized alternative to Type 304. In the case of 347, تاہم, the stabilizing agent is columbium. This metal intensifies 347’s already present ability to withstand intergranular corrosion for maximum capabilities. Additionally, the columbium allows for 347 to undergo repeated heating in temperatures up to 1650° F. As a result, the metal is commonly applied to high temperature equipment, such as gaskets and expansion joints, along with rocket engine and chemical manufacturing.
In addition to its heat resistance properties, 347 also enjoys better resistance against creep and stress rupture corrosions. This is another advantage of type 304, as 347’s characteristics may be better suited for environments where stabilization is a primary concern.
قسم 347 is known for being workable under all common welding techniques, along with hot and cold working. تاہم, when being heat treated the metal must be heated up in the range of 2100 to 2250°F. This is due to 347’s inability to work harden under heat treatment. Cold reduction is the only method that will utilize the alloy’s elevated properties.
347 سٹینلیس سٹیل 1.4550 تیار شدہ مصنوعات کا فارم
- Round, Sqaure, Hexagon & Flat Bars
- Seamless / Welded Pipes
- Seamless / Welded Tubes
- Hot & Cold Rolled Plates & Sheets
- Forged Bars
- Buttweld Pipe Fittings
- Forged Fittings
- Ferrule Compression Fittings
- Forged Flanges
- Valves
- Guages
کے لیے درخواستیں 347 سٹینلیس سٹیل
Collector rings, airplane exhaust stacks, annealing box covers, jet engine parts.expansion joints, tubing, fasteners, flexible metal hose and bellows
ایگریڈ کے مساوی 347
یورپی یونین میں | USA – | فرانس افنور | انگلینڈ بی ایس | سویڈن ایس ایس | روس GOST |
X6CrNiNb18-10 | 347 | Z6CNNb18-10 | 347S31 | 2338 | 08KH18N12B |
کمپوزیشن کے لیے حدود 347 سٹینلیس سٹیل کا گریڈ
گریڈ | میں | Mn | پی | سی | ایس | اور | کروڑ | OTHER | ن | |
347 | منٹ. | 9.00 | – | – | – | – | – | 17.0 | Nb=10(C+N) | – |
زیادہ سے زیادہ. | 13.00 | 2.00 | 0.045 | 0.08 | 0.030 | 1.00 | 20.0 | 1.0 |
مکینیکل پراپرٹیز
گریڈ | تناؤ کی طاقت (ایم پی اے) منٹ | لمبا ہونا (% in 50mm) منٹ | پیداوار کی طاقت 0.2% ثبوت (ایم پی اے) منٹ | سختی | |
راک ویل بی (HR B) زیادہ سے زیادہ | برنیل (ایچ بی) زیادہ سے زیادہ | ||||
347 | 515 | 40 | 205 | 92 | 201 |
فزیکل پراپرٹیز
گریڈ | کثافت (kg/m3) | Elastic Modulus (جی پی اے) | Mean Coefficient of Thermal Expansion (m/m/0C) | تھرمل چالکتا (W/m.K) | Specific Heat 0-1000C (J/kg.K) | برقی مزاحمتی صلاحیت (n.m) | |||
0-1000سی | 0-3150سی | 0-5380سی | at 1000C | at 5000C | |||||
347 | 8000 | 193 | 17.2 | 17.8 | 18.4 | 16.2 | 21.5 | 500 | 720 |
سنکنرن مزاحمت
- Pitting corrosion-resistant steel
- Steel resistant to rural and non-industrial urban atmosphere
- Stainless steel less aggressive sea atmosphere
- Steel resistant to salt of nitric acid and nitric acid at concentrations of up to 55% and temperatures up to 80 °C
- Steel resistant to non-oxidizing environments, e.g. H2SO4, HCl, HF, وغیرہ.
- Steel resistant to stress corrosion in solutions of chlorides and hydroxides
- Steel resistant to pitting and contact corrosion in environments containing halides
گرمی کا علاج
Annealing temperature range is 1800 to 2000°F
May be stress relief annealed within the carbide precipitation range of 800 to 1500°F without any danger of subsequent intergranualr corrosion
Cannot be hardened by heat treatment
WELDABILITY
Austenitic stainless steels are considered to be the most weldable out of all high alloy steels
Can be welded by all fusion and resistance welding processes